Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hot-Working Temperature 801.7 °C
1475 °F
Slow heating
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Hot-Working Temperature 801.7 °C
1475 °F
Slow heating
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..
Hot-Working Temperature 801.7 °C
1475 °F
Slow heating
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..