Processing Properties Metric English Comments
Hot-Working Temperature 649 - 704 °C
1200 - 1300 °F
Mueller Alloy 3770 Forging Brass (UNS C37700)
General forging applicationsApplications: Alloy 3770 is used as rod base stock for press and hammer forgings requiring the excellent corrosion resistance and machinability of brass. Typical applica..
Hot-Working Temperature 649 °C
1200 °F
Flow Stress of 25 MP at 3.6s<sup>-1<sup>
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar
Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope..
Hot-Working Temperature 649 °C
1200 °F
Flow Stress of 40 MP at 3.6s<sup>-1<sup>
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..