Mueller Alloy 3770 Forging Brass (UNS C37700)

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Mueller Industries Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mueller Alloy 3770 Forging Brass (UNS C37700).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General forging applicationsApplications: Alloy 3770 is used as rod base stock for press and hammer forgings requiring the excellent corrosion resistance and machinability of brass. Typical applications include valve bodies, hardware, fittings and miscellaneous brass forgings.Information Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 78
78
Tensile Strength at Break 359 MPa
52000 psi
Tensile Strength, Yield 138 MPa
20000 psi
Elongation at Break 45 %
45 %
Machinability 90 %
90 %
UNS C36000 = 100%
Component Elements Properties Metric English Comments
Copper, Cu 58 - 61 %
58 - 61 %
Iron, Fe <= 0.30 %
<= 0.30 %
Lead, Pb 1.5 - 2.5 %
1.5 - 2.5 %
Zinc, Zn 36.2 - 40.5 %
36.2 - 40.5 %
Remainder
Processing Properties Metric English Comments
Processing Temperature 260 °C
500 °F
Stress Relieving
Hot-Working Temperature 649 - 704 °C
1200 - 1300 °F