Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Cooling Temperature | 190 - 210 °C | 374 - 410 °F | 6 |
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Die Cooling Temperature | 190 - 210 °C | 374 - 410 °F | TIP, 7 |
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |