Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical properties.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ISO 868
Tensile Strength, Yield 35.00 MPa
5076 psi
ISO 527-2/5A/500
Elongation at Break 650 %
650 %
ISO 527-2/5A/500
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
100% Modulus 0.00600 GPa
0.870 ksi
ISO 527-2/5A/500
300% Modulus 0.01100 GPa
1.595 ksi
ISO 527-2/5A/500
Tear Strength 90.3 kN/m
515 pli
ISO 34-1B
Abrasion 25
25
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ISO 306
Processing Properties Metric English Comments
Zone 1 175 - 195 °C
347 - 383 °F
Zone 2 185 - 205 °C
365 - 401 °F
Zone 3 195 - 215 °C
383 - 419 °F
Zone 4 200 - 220 °C
392 - 428 °F
Adapter Temperature 200 - 220 °C
392 - 428 °F
5
Die Cooling Temperature 190 - 210 °C
374 - 410 °F
6
190 - 210 °C
374 - 410 °F
TIP, 7
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F