Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.1524 cm | 0.06000 in | |
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu.. |
|||
Die Opening | 0.1524 cm | 0.06000 in | |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |
|||
Die Opening | 0.1524 cm | 0.06000 in | |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
Die Opening | 0.1524 cm | 0.06000 in | |
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended .. |