Polymer Property : Die Opening = 0.04000 in Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Opening 0.1016 - 0.127 cm
0.04000 - 0.0500 in
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade
ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati..
Die Opening 0.1016 cm
0.04000 in
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin
Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation ..
Die Opening 0.1016 cm
0.04000 in
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b..