Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 34.3 - 120 MPa | 4980 - 17400 psi | Average value: 83.1 MPa Grade Count:17 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |