Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 3000 - 7000 MPa | 435000 - 1.02e+6 psi | Injection |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |