Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 951.7 - 1010 °C | 1745 - 1850 °F | Brazing Range |
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy Applications:Premabraze 130 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |
|||
Processing Temperature | 951.7 - 1010 °C | 1745 - 1850 °F | Brazing Range |
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy Applications:Premabraze 131 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |