Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 788 - 927 °C | 1450 - 1700 °F | Brazing Range |
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into.. |
|||
Processing Temperature | 788 - 927 °C | 1450 - 1700 °F | Brazing Range |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Processing Temperature | 788 - 927 °C | 1450 - 1700 °F | Brazing Range |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |