Processing Properties Metric English Comments
Processing Temperature 788 - 927 °C
1450 - 1700 °F
Brazing Range
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal
Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into..
Processing Temperature 788 - 927 °C
1450 - 1700 °F
Brazing Range
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Processing Temperature 788 - 927 °C
1450 - 1700 °F
Brazing Range
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Processing Temperature 788 °C
1450 °F
Brazing
Cadi 2 MOLD-MOR™
A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an..
Processing Temperature 788 °C
1450 °F
Brazing
Cadi 20 MOLD-MOR™
A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company.
Processing Temperature 788 °C
1450 °F
Brazing
Cadi C17500 Copper Alloy
Information provided by Cadi Company.
Copyright © lookpolymers.com All Rights Reserved