Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 71.0 - 91.0 °C @Time 576 sec |
160 - 196 °F @Time 0.160 hour |
Immersion |
Henkel Turco C 2087X Cleaner Turco C 2087X is a single package liquid cleaner formulated for the removal of lubricants and other drawing compounds or oils from baskets, racks, tumbling barrels and production parts. The cleaner .. |