Polymer Property : Processing Temperature = 196 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 71.0 - 91.0 °C

@Time 576 sec
160 - 196 °F

@Time 0.160 hour
Immersion
Henkel Turco C 2087X Cleaner
Turco C 2087X is a single package liquid cleaner formulated for the removal of lubricants and other drawing compounds or oils from baskets, racks, tumbling barrels and production parts. The cleaner ..