Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 88.9 °C
192 °F
Seal Initiation Temp
M. Holland Company MAGMA® LM233-A LLDPE  (discontinued **)
Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland.