Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company MAGMA® LM233-A LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company MAGMA® LM233-A LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 12.7 cm
5.00 in
at 280°C, 1.0 mil
Thermal Properties Metric English Comments
Melting Point 97.2 °C
207 °F
ASTM D3218
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ASTM D1003
Gloss 94 %
94 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 88.9 °C
192 °F
Seal Initiation Temp
Feed Temperature <= 149 °C
<= 300 °F
Melt Temperature 182 - 199 °C
360 - 390 °F
302 °C
575 °F
Suggested for extrusion coating only
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0
Descriptive Properties Value Comments
Adhesion to PP Films 0.98
at 280°C
Form Pellets