Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 430 °C | 806 °F | Typical Firing Temperature; Typical Firing Time: 10 min. |
Ferro EG 2018 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |