Polymer Property : Processing Temperature = 430 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 430 °C
806 °F
Typical Firing Temperature; Typical Firing Time: 10 min.
Ferro EG 2018 Display Device
Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and ..