Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 743 - 843 °C | 1370 - 1550 °F | Brazing Range |
Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in.. |
|||
Processing Temperature | 743 - 840.6 °C | 1370 - 1545 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A35 Brazing Alloy Silvaloy A35 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is used for brazing in the electrical industry and for brazing brass.. |
|||
Processing Temperature | 743 - 843 °C | 1370 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A45 Brazing Alloy Silvaloy A45 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in the electrical industry and for brazing .. |
|||
Processing Temperature | 743 - 843 °C | 1370 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A45 Flux Coated Rod Brazing Alloy Silvaloy A45 FC is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in electrical industry and for brazing b.. |
|||
Processing Temperature | 743 - 843 °C | 1370 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A50 Brazing Alloy Silvaloy A50 is widely used for brazing in the electrical industry, as well as in the dairy and food industries where the use of cadmium-containing filler metals is prohibited. Silvaloy A50 has a br.. |