Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 100 - 390 °C | 212 - 734 °F | Average value: 360 °C Grade Count:21 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Processing Temperature | 343 - 390 °C | 650 - 734 °F | Average value: 370 °C Grade Count:5 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |