Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 732 - 843 °C
1350 - 1550 °F
Brazing Range
Lucas-Milhaupt FOS FLO 7 Copper Phosphorus Alloy
Applications:Fos-Flo 7 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service..
Processing Temperature 732 - 843 °C
1350 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvabraze 33830 Brazing Alloy
Silvabraze is used for brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten, and molybdenum. It is primarily used for the joining of copper-to-copper on vib..
Processing Temperature 732 - 799 °C
1350 - 1470 °F
Brazing Temperature
Lucas-Milhaupt Silvalite Brazing Alloy
SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v..
Processing Temperature 732 - 843 °C
1350 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 0 Brazing Alloy
Silvaloy 0 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on ..