Polymer Property : Processing Temperature = 690.6 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 690.6 - 788 °C
1275 - 1450 °F
Brazing Range
Lucas-Milhaupt SIL-FOS 6 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 6 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi..