Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 690.6 - 788 °C | 1275 - 1450 °F | Brazing Range |
Lucas-Milhaupt SIL-FOS 6 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 6 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |