Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 25.0 - 27.0 °C | 77.0 - 80.6 °F | Average value: 26.2 °C Grade Count:13 |
Overview of materials for Silicone, RTV, Construction Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values.. |