Polymer Property : Processing Temperature = 2370 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 1300 °C
2370 °F
Typical Firing Temperature
Ferro EG 2410 Specialty Glass
Glass Type: Si-MG-Al Typical Powder Form: MVG Typical Application: Sintering Aid / Glaze Ferro offers a wide range of compositions for specialty applications including sintering aids used in the gl..
Processing Temperature 1300 °C
2370 °F
Typical Firing Temperature
Ferro EG 2705 Glaze and Sealant Glass
Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat..
Processing Temperature 1300 °C
2370 °F
Typical Firing Temperature
Ferro EG 0002 Glazes and Sealants
Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin..