Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 111 °C | 232 °F | Seal Initiation temperature |
Dow Elite® 5110 Linear Low Density Polyethylene 5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin.. |