Polymer Property : Processing Temperature = 111 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 111 °C
232 °F
Seal Initiation temperature
Dow Elite® 5110 Linear Low Density Polyethylene
5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin..