Processing Properties Metric English Comments
Processing Temperature 900.0 °C
1652 °F
Firing Temp
Wieland ALLUX®/ZIROX® Ceramic Veneering
Veneering ceramic with a leucite-free HDAM™ microstructure. Extremely homogeneous, gingiva friendly and plaque resistant surface.Applications: ceramic veneeringDental
Processing Temperature 900.0 °C
1652 °F
Flow Temp
Wieland Porta Optimum 900 Solder
Solder supplied as strip (0.18 oz. roll)Information provided by WielandDental
Processing Temperature 900.0 °C
1652 °F
Firing Temp
Wieland REFLEX® Ceramic Veneering
Innovative veneering ceramic with extremely smooth, homogeneous and plaque resistant surface. Also, it is gingiva and antagonist friendly as well as chairside polishable. The opalescence remains s..