Wieland Porta Optimum 900 Solder

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Wieland
Trade Name Porta
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Porta Optimum 900 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solder supplied as strip (0.18 oz. roll)Information provided by WielandDental
Component Elements Properties Metric English Comments
Gold, Au 88.7 %
88.7 %
Iridium, Ir 0.10 %
0.10 %
Platinum, Pt 2.0 %
2.0 %
Silver, Ag 3.0 %
3.0 %
Zinc, Zn 6.2 %
6.2 %
Processing Properties Metric English Comments
Processing Temperature 900.0 °C
1652 °F
Flow Temp
Melt Temperature 830.0 - 890.0 °C
1526 - 1634 °F
Descriptive Properties Value Comments
Color yellow