Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.47 J/g-°C @Temperature 260 °C |
0.590 BTU/lb-°F @Temperature 500 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |