Thermal Properties Metric English Comments
Specific Heat Capacity 2.47 J/g-°C

@Temperature 260 °C
0.590 BTU/lb-°F

@Temperature 500 °F
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..