Thermal Properties Metric English Comments
Specific Heat Capacity 1.84 J/g-°C

@Temperature -17.8 °C
0.440 BTU/lb-°F

@Temperature 0.000 °F
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..
Specific Heat Capacity 1.84 J/g-°C

@Temperature -17.8 °C
0.440 BTU/lb-°F

@Temperature 0.000 °F
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 200 °C
0.440 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 200 °C
0.440 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 150 °C
0.440 BTU/lb-°F

@Temperature 302 °F
DSC
Eastman Cadence™ GS1 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 150 °C
0.440 BTU/lb-°F

@Temperature 302 °F
DSC
Eastman Cadence™ GS2 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 150 °C
0.440 BTU/lb-°F

@Temperature 302 °F
DSC
Eastman Cadence™ GS3 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 150 °C
0.440 BTU/lb-°F

@Temperature 302 °F
DSC
Eastman Cadence™ GS4 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 20.0 °C
0.440 BTU/lb-°F

@Temperature 68.0 °F
Dow SPECFLEX™ NC 630 Polyol
SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082..
Specific Heat Capacity 1.84 J/g-°C

@Temperature 20.0 °C
0.440 BTU/lb-°F

@Temperature 68.0 °F
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt..