Polymer Property : Specific Heat Capacity = 1.62 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.62 J/g-°C

@Temperature 200 °C
0.387 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Specific Heat Capacity 1.62 J/g-°C

@Temperature 200 °C
0.387 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Specific Heat Capacity 1.62 J/g-°C

@Temperature 200 °C
0.387 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Specific Heat Capacity 1.62 J/g-°C

@Temperature 200 °C
0.387 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Copyright © lookpolymers.com All Rights Reserved