Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.34 J/g-°C @Temperature 60.0 °C |
0.320 BTU/lb-°F @Temperature 140 °F |
|
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Specific Heat Capacity | 1.34 J/g-°C @Temperature 50.0 °C |
0.320 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Specific Heat Capacity | 1.34 J/g-°C @Temperature 300 °C |
0.320 BTU/lb-°F @Temperature 572 °F |
By DSC |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Specific Heat Capacity | 1.34 J/g-°C @Temperature 50.0 °C |
0.320 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Specific Heat Capacity | 1.34 J/g-°C @Temperature 60.0 °C |
0.320 BTU/lb-°F @Temperature 140 °F |
DSC |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |