Thermal Properties Metric English Comments
Specific Heat Capacity 1.34 J/g-°C

@Temperature 60.0 °C
0.320 BTU/lb-°F

@Temperature 140 °F
Eastman EASTALLOY Polymer DA105, Natural Alloy  (discontinued **)
General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma..
Specific Heat Capacity 1.34 J/g-°C

@Temperature 50.0 °C
0.320 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Specific Heat Capacity 1.34 J/g-°C

@Temperature 300 °C
0.320 BTU/lb-°F

@Temperature 572 °F
By DSC
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Specific Heat Capacity 1.34 J/g-°C

@Temperature 50.0 °C
0.320 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Specific Heat Capacity 1.34 J/g-°C

@Temperature 60.0 °C
0.320 BTU/lb-°F

@Temperature 140 °F
DSC
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..