Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.33 J/g-°C @Temperature 50.0 °C |
0.318 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Specific Heat Capacity | 1.33 J/g-°C @Temperature 50.0 °C |
0.318 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Specific Heat Capacity | 1.33 J/g-°C @Temperature 50.0 °C |
0.318 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |