Polymer Property : Specific Heat Capacity = 1.10 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-105C PET Bottle Grade
A co-polymer used for soft drinks and other applications.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-109JS PET Sheet Grade
Used mainly for 5 to 20 liter mineral water containers
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-113C PET Sheet Grade
Used mainly for box strapping.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET D-101-SH Monofilament Resin
Used in the paper industry as paper pulp nets.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET F097H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET F097HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET FR-101-H Monofilament Resin
Used as textile grade flame retardant for furniture, car and plane upholstery.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-101C PET Sheet Grade
A sheet grade polymer used in thick films.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B101H Monofilament Resin
Generally used in monofilament v-belts, zips and other technical applications.
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
Pearl Engineering PEPLPET B-103C PET Bottle Grade
A co-polymer used for mineral water bottles
Specific Heat Capacity 1.10 J/g-°C

@Temperature 23.0 °C
0.263 BTU/lb-°F

@Temperature 73.4 °F
Kuraray Vectran® HT 1500/300 LCP Fiber
 is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an..