Thermal Properties Metric English Comments
Specific Heat Capacity 0.725 J/g-°C

@Temperature 399 °C
0.173 BTU/lb-°F

@Temperature 750 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..