Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.724 J/g-°C @Temperature 60.0 °C |
0.173 BTU/lb-°F @Temperature 140 °F |
Vapor (1atm) |
Asahi Glass ASAHIKLIN AK-225 Hydrochlorofluorocarbon Solvent Asahilkin AK-225 is an environmentally sensible hydrochlorofluorocarbon (HCFC) designed to replace chlorofluorocarbon (CFC), perfluorocarbon (PFC), and other HCFCs with high ODP values in a variety .. |
|||
Specific Heat Capacity | 0.725 J/g-°C @Temperature 399 °C |
0.173 BTU/lb-°F @Temperature 750 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |