Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.644 J/g-°C @Temperature 900 °C |
0.154 BTU/lb-°F @Temperature 1650 °F |
|
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |