Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.154 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.644 J/g-°C

@Temperature 900 °C
0.154 BTU/lb-°F

@Temperature 1650 °F
Latrobe CSS-42Lâ„¢ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel
CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness ..