Thermal Properties Metric English Comments
Specific Heat Capacity 2.00 J/g-°C

@Temperature 200 °C
0.478 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 240 °C
0.478 BTU/lb-°F

@Temperature 464 °F
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 150 °C
0.478 BTU/lb-°F

@Temperature 302 °F
solid; DSC
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 150 °C
0.478 BTU/lb-°F

@Temperature 302 °F
solid; DSC
Eastman Eastman AP006 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 150 °C
0.478 BTU/lb-°F

@Temperature 302 °F
solid; DSC
Eastman Eastman AP007 Copolyester
Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 100 °C
0.478 BTU/lb-°F

@Temperature 212 °F
Dow VORALUX™ HL 430 Copolymer Polyol
VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 60.0 °C
0.478 BTU/lb-°F

@Temperature 140 °F
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt..
Specific Heat Capacity 2.00 J/g-°C

@Temperature 200 °C
0.478 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..