Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.463 J/g-°C @Temperature 23.0 °C |
0.111 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |