Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 22.8 °C |
0.108 BTU/lb-°F @Temperature 73.0 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a.. |