Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.448 J/g-°C @Temperature 22.8 °C |
0.107 BTU/lb-°F @Temperature 73.0 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |