Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.107 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.448 J/g-°C

@Temperature 22.8 °C
0.107 BTU/lb-°F

@Temperature 73.0 °F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.448 J/g-°C

@Temperature 200 °C
0.107 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.448 J/g-°C

@Temperature 200 °C
0.107 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 23.0 °C
0.107 BTU/lb-°F

@Temperature 73.4 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..
Specific Heat Capacity 0.448 J/g-°C

@Temperature 200 °C
0.107 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.448 J/g-°C

@Temperature 200 °C
0.107 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Specific Heat Capacity 0.449 J/g-°C

@Temperature 400 °C
0.107 BTU/lb-°F

@Temperature 752 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Specific Heat Capacity 0.447 J/g-°C

@Temperature 20.0 °C
0.107 BTU/lb-°F

@Temperature 68.0 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..
Copyright © lookpolymers.com All Rights Reserved