Specific Heat Capacity 0.431 J/g-°C

@Temperature 400 °C
0.103 BTU/lb-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked
Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.431 J/g-°C

@Temperature 400 °C
0.103 BTU/lb-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked
Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.431 J/g-°C

@Temperature 400 °C
0.103 BTU/lb-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked
Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.431 J/g-°C

@Temperature 400 °C
0.103 BTU/lb-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked
Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.431 J/g-°C

@Temperature 400 °C
0.103 BTU/lb-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.