Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.421 J/g-°C @Temperature 20.0 °C |
0.101 BTU/lb-°F @Temperature 68.0 °F |
|
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |