Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
hardened and tempered condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
hardened and tempered condition |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |