Thermal Properties Metric English Comments
Specific Heat Capacity 0.406 J/g-°C

@Temperature 0.000 °C
0.0970 BTU/lb-°F

@Temperature 32.0 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.406 J/g-°C

@Temperature 0.000 °C
0.0970 BTU/lb-°F

@Temperature 32.0 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.406 J/g-°C

@Temperature 200 °C
0.0970 BTU/lb-°F

@Temperature 392 °F
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked
Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.406 J/g-°C

@Temperature 200 °C
0.0970 BTU/lb-°F

@Temperature 392 °F
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked
Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.406 J/g-°C

@Temperature 200 °C
0.0970 BTU/lb-°F

@Temperature 392 °F
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked
Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.406 J/g-°C

@Temperature 200 °C
0.0970 BTU/lb-°F

@Temperature 392 °F
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked
Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.406 J/g-°C

@Temperature 0.000 °C
0.0970 BTU/lb-°F

@Temperature 32.0 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.406 J/g-°C

@Temperature 0.000 °C
0.0970 BTU/lb-°F

@Temperature 32.0 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.406 J/g-°C

@Temperature 200 °C
0.0970 BTU/lb-°F

@Temperature 392 °F
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.